Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 440 - 560 MPa
63800 - 81200 psi
Tensile Strength, Yield 370 - 520 MPa
53700 - 75400 psi
Elongation at Break 2.0 - 20 %
2.0 - 20 %
Modulus of Elasticity 138 GPa
20000 ksi
Machinability 40 %
40 %
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Melting Point 1010 - 1050 °C
1850 - 1920 °F
Solidus 1010 °C
1850 °F
Liquidus 1050 °C
1920 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.40 - 0.70 %
0.40 - 0.70 %
Cobalt, Co 2.4 - 2.7 %
2.4 - 2.7 %
Copper, Cu 97 %
97 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000570 - 0.00000860 ohm-cm
0.00000570 - 0.00000860 ohm-cm
20-30% IACS Conductivity
Users viewing this material also viewed the following: