| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.91 g/cc <br>@Temperature 25.0 °C |
0.105 lb/in³ <br>@Temperature 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Elasticity | 59.0 GPa | 8560 ksi | |
| Poissons Ratio | 0.24 | 0.24 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 4.40 µm/m-°C <br>@Temperature 20.0 - 300 °C |
2.44 µin/in-°F <br>@Temperature 68.0 - 572 °F |
ISO 7991 |
| Thermal Conductivity | 0.900 W/m-K <br>@Temperature 90.0 °C |
6.25 BTU-in/hr-ft²-°F <br>@Temperature 194 °F |
|
| Transformation Temperature, Tg | 549 °C | 1020 °F | ISO 7884-8 |
| Softening Point | 736 °C | 1360 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
| Working Point | 1034 °C | 1893 °F | Viscosity 10<sup>4</sup> dPa s; ISO 7884-2 |
| Annealing Point | 540 °C | 1000 °F | Viscosity 10<sup>13</sup> dPa s; ISO 7884-4 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.552 <br>@Wavelength 587.6 nm |
1.552 <br>@Wavelength 587.6 nm |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+10 ohm-cm <br>@Temperature 350 °C |
1.00e+10 ohm-cm <br>@Temperature 662 °F |
|
| 1.60e+11 ohm-cm <br>@Temperature 250 °C |
1.60e+11 ohm-cm <br>@Temperature 482 °F |
||
| Dielectric Constant | 6.0 <br>@Frequency 1.00e+6 Hz,<br> Temperature 25.0 °C |
6.0 <br>@Frequency 1.00e+6 Hz,<br> Temperature 77.0 °F |
|
| Dielectric Loss Index | 0.0031 <br>@Frequency 1.00e+6 Hz,<br> Temperature 25.0 °C |
0.0031 <br>@Frequency 1.00e+6 Hz,<br> Temperature 77.0 °F |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 4 | 4 | DIN 12116 |
| Alkali Class, AR | 3 | 3 | ISO 695 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Hydrolytic Resistance | Class HGB 1 | ISO 719 |
| Stress-optical Coefficient K (10-6mm2N-1) | 3.6 | DIN 52314 |