Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N330 (HAF) Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N330 (HAF) Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5N330 (HAF)40All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Yield 23.8 MPa
3450 psi
Elongation at Yield 389 %
389 %
100% Modulus 0.007053 GPa
1.023 ksi
200% Modulus 0.01556 GPa
2.257 ksi
300% Modulus 0.02268 GPa
3.289 ksi
Tear Strength 63.2 kN/m
361 pli
Die C
Taber Abrasion, mg/1000 Cycles 0.10
0.10
H-18, mg loss/rev
Compression Set 56 %

@Temperature 70.0 °C,
Time 79200 sec
56 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 149 °C
0.333 hour

@Temperature 300 °F