Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 44.1 MPa
6400 psi
5 mm/min; ASTM D638
Flexural Strength 66.7 MPa
9670 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.16 GPa
313 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 1.86 J/cm

@Thickness 3.17 mm
3.49 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C
210 °F
B/50; ISO R306