Samsung Cheil Industries Starex® SV-0157 ABS, Unreinforced Extrusion Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SV-0157 ABS, Unreinforced Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 5.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Flexural Strength 53.9 MPa
7820 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.55 J/cm

@Thickness 6.35 mm
4.78 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.60 - 6.00 mm
HB

@Thickness 0.0630 - 0.236 in
Users viewing this material also viewed the following: