Multibase Multi-Flex® TPE A 7699 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 7699 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Multi-Flex® A 7699 is an acoustic barrier compound for medium density applications . Multi-Flex® TPE compounds are based on Shell Kraton G polymers licensed to Multibase. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0052 cm/cm
0.0052 in/in
ASTM D955
Melt Flow 1.7 g/10 min
1.7 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
10 sec; ASTM D-2240
Tensile Strength, Ultimate 2.30 MPa
334 psi
ASTM D412
Elongation at Break 225 %
225 %
ASTM D412
Flexural Modulus 0.0372 GPa
5.40 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 25.4 kN/m
145 pli
ASTM D624