Polymer Property : Tensile Strength, Yield = 5830 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.2 MPa
5830 psi
ASTM D638
PolyMirae Moplen HP620M CPP Film Grade Polypropylene
Moplen HP620M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP620M is suitable for rigid core resin of CPP. Moplen HP620M res..
Tensile Strength, Yield 40.2 MPa
5830 psi
ASTM D638
Hyosung Topilene J301CP PP
J301CP Injection Special Purpose GradeApplications: Cap of pressure bottleCharacteristics:High stiffnessSlip propertyInformation provided by Hyosung Corporation
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical HIPS MI750L PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Tensile Strength, Yield 40.2 MPa
5830 psi
ASTM D638
Hyosung Topilene J801 PP
J801 Injection Special Purpose GradeApplications:Disposable syringeTransparent productCharacteristics:TransparencyHigh stiffnessInformation provided by Hyosung Corporation
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced
Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® GC-0710 ABS/PET, Unreinforced Recycled
Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced
WNP GradeInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SV-0157 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced
Used in electric goods etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced
Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® GC-0710 ABS/PET, Unreinforced Recycled
Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced
WNP GradeInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SV-0157 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced
Used in electric goods etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 40.2 MPa
5830 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SBB 3715 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1, 5 mm/min speed; ASTM D-638
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1; 5mm/min speed; ASTM D638
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1; ASTM D-638
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1; ASTM D-638
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1, 5 mm/min speed; ASTM D-638
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1; 5mm/min speed; ASTM D638
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1, 5 mm/min speed; ASTM D-638
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
Type 1, 5 mm/min speed; ASTM D-638
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali