Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tygon S3â„¢ B-44-4X, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Tygon S3â„¢ line combines the high performance standards customers demand with an eco-friendly tubing design. Tygon S3â„¢ Food, Milk and Dairy Tubing offers dependable performance in countless filling, draining, transfer and processing applications. Its smooth, non-porous bore inhibits particle entrapment, promoting a sanitary fluid path by minimizing potential for bacterial growth. It has outstanding resistance to harsh alkaline cleaners and is equally unaffected by commonly used sanitizers. Non-toxic, taste-free and odor-free, Tygon S3â„¢ Food, Milk and Dairy Tubing meets applicable regulatory standards for contact with food products. Complete clarity for positive visual inspection and flow control, it is available in up to a 6" inside diameter, making it a flexible replacement for rigid piping systems. Applications Aseptic filling Condiment dispensing Dairy processing Soft-serve dispensing Vitamin and flavor concentrate systems Features and Benefits Smooth, non-porous bore will not trap particulates or promote bacterial growth Compatible with foods containing a high oil content Resistant to harsh alkaline cleaners and sanitizers Excellent alternative to rigid piping systems Contains no BPA or phthalates Regulatory Information: Tygon S3â„¢ complies with FDA, NSF, 3-A, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EC for many foods and beverages. Tygon S3â„¢ tubing products do not contain chemicals listed in California's Prop 65. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.22 %

@Temperature 22.8 °C,
Time 86400 sec
0.22 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 15.0 sec
66

@Time 0.00417 hour
ASTM D2240
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Tensile Strength, Yield 9.508 MPa

@Strain 200 %
1379 psi

@Strain 200 %
Elongation at Break 390 %
390 %
ASTM D412
Tear Strength 43.8 kN/m
250 pli
ASTM D1004
Compression Set 59 %

@Temperature 70.0 °C,
Time 79200 sec
59 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 57 %
57 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -35.6 °C
-32.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Clear
Users viewing this material also viewed the following: