Saint-Gobain Tygon® Norprene® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® Norprene® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Good for use in clean-in-place and steam-in-place cleaning and sterilization systems, Norprene® Pressure Tubing has excellent alkali resistance and is compatible with numerous oxidizing agents such as hydrogen peroxide, sodium hypochlorite and ozone. Norprene® Pressure Tubing fully complies with FDA 177.2600 criteria, 3A Sanitary Standards and NSF Standard 51, which are applicable to many food contact applications. Norprene® Pressure Tubing exhibits excellent resistance to ozone and UV light, with little or no signs of deterioration in laboratory testing equivalent to 10 years of outdoor exposure. Norprene® Pressure Tubing provides long service life when exposed to heat, abrasion and pressure. It is temperature resistant up to 275°F and retains flexibility to -60°F. Features and Benefits Handles at least 4 times the pressure of non-reinforced tubing Temperature resistant from -60°F to 275°F Ozone and UV light resistant Repeatedly autoclavable Chemically compatible with a wide range of fluids Meets FDA, 3A and NSF Criteria Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792-00
Water Absorption 0.30 %

@Temperature 22.8 °C,
Time 86400 sec
0.30 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore A 61

@Time 15.0 sec
61

@Time 0.00417 hour
ASTM D2240-03
Tensile Strength 6.89 MPa
1000 psi
ASTM D412-98
Elongation at Break 375 %
375 %
ASTM D412-98
100% Modulus 0.00283 GPa
0.410 ksi
ASTM D412-98
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-98
Tear Strength 21.0 kN/m
120 pli
ASTM D1004-03
Compression Set 30 %

@Temperature 70.0 °C,
Time 79200 sec
30 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395-03 Method B
Tensile Set 57 %
57 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-98
Electrical Properties Metric English Comments
Dielectric Strength 21.1 kV/mm
535 kV/in
ASTM D149-97
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Cream