Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam

Category Polymer , Adhesive , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Closed cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side. The high-tack positioning adhesive grips tight on initial contact and keeps foam in place during assembly. The liner on the non-adhesive side keeps slit rolls from falling apart.Features/Benefits:Excellent for light, dust, moisture seal and all general sealing needsClosed cell content develops positive seal at only 30% compressionRolls are dimensionally stable--will not ooze, drop or run under compressionEasy to radius, enhancing positive seal on curved surfacesLow thermal conductivity improves the energy efficiency of structureControls sound transmission and vibration--ideal for acoustical partitionsLow deflection force reduces distortion of adjacent materialTypical Applications: Acoustical partitions, suspended ceilings, cold rooms, vending machines, culvert pipes, hot tubs, seals for flashing, saunas, computer cabinet dust and noise seal, roof top air conditioner insulation, dust seal on analytic equipment. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/8" to 3/4".) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.0969 g/cc
0.00350 lb/in³
ASTM D1667
Water Absorption 4.0 %
4.0 %
% by volume; NTP-35
Mechanical Properties Metric English Comments
Hardness, Shore OO 13
13
ASTM D2240
Tensile Strength, Yield 0.103 MPa
15.0 psi
ASTM D-412 (Die A)
Elongation at Break 140 %
140 %
ASTM D-412 (Die A)
Compressive Strength 0.00758 MPa
1.10 psi
Compression Deflection, Compressed to 30%.; ASTM D1667
Compressive Modulus 0.0000138 GPa
0.00200 ksi
Force to Compress, Value for 30% compression.
Compression Set 7.0 %
7.0 %
Constant Deflection, Compressed to 30%.; Norton Test Procedure 37
Thermal Properties Metric English Comments
Thermal Conductivity 0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
ASTM-C-518
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -26.1 °C
-15.0 °F
Descriptive Properties Value Comments
Color Gray