Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain COHRlastic® 200A Silicone Sponge/Aggressive Acrylic Adhesive Pressure Sensitive Tape

Category Polymer , Adhesive , Tape , Thermoset , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name COHRlastic®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain COHRlastic® 200A Silicone Sponge/Aggressive Acrylic Adhesive Pressure Sensitive Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Strip-N-Stick® tape provides all the benefits of silicone rubber in an easy-to-apply, pressure-sensitive adhesive tape form. Compressible and flexible, it can conform to irregular surfaces, wrap over cylinders or be formed to produce right angles. Applications include gasketing, vibration damping, and thermal insulation. The tape reduces the need for expensive die-cut-parts--you don't pay for the center. It also eliminates the high cost of bonding and will be slit to order for 1/2" and up. 200A is a silicone sponge with aggressive acrylic adhesive. Adhesive temperature range for Silicone PSA is -100°F to +500°F and for Acrylic PSA, -20°F to 300°F. Base material is R10470M. Silicone rubber material type is sponge. Adhesive type is acrylic. All data based on a 0.0625 inch test sample.(Other thicknesses available.) Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.448 MPa
65.0 psi
ASTM D412
Elongation at Break 150 %
150 %
ASTM D412
Compressive Strength 0.0689 MPa
10.0 psi
Compression Deflection, Compressed to 75% original thickness.; ASTM D1056
Compression Set 25 %

@Temperature 100 °C
25 %

@Temperature 212 °F
Constant Deflection, Compressed 50% for 22 hrs; ASTM D1056
Descriptive Properties Value Comments
Color Orange-Tan