Eliokem Chemigum® P7400 Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eliokem
Trade Name Chemigum®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eliokem Chemigum® P7400 Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose for halogen-free blends. 33% bound ACN. Crosslinked polymer structure. CaCO3 partitioning agent.Can be used in TPU blends.Used in footwear and cable jacketing.Information provided by Eliokem.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Particle Size 1200 µm
1200 µm
Median
Mooney Viscosity 55

@Temperature 100 °C
55

@Temperature 212 °F
ML 1+4