SGL Carbon Group SIGRAFIL C® C25 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer SGL Carbon Group
Trade Name SIGRAFIL C®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group SIGRAFIL C® C25 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIGRAFIL C fibers can be added to thermoplastic injection molding compounds and are also available in a pelletized form for improved handling characteristics. SIGRAFIL C fibers are optimized in terms of their mechanical properties to offer excellent physical handling and process feeding properties. SIGRAFIL C can be blended with a variety of resins.Information provided by SGL Carbon Group
Physical Properties Metric English Comments
Bulk Density 0.230 g/cc
0.00831 lb/in³
Density 1.80 g/cc
0.0650 lb/in³
Fiber Density
Filament Diameter 7.5 µm
7.5 µm
Mechanical Properties Metric English Comments
Tensile Strength at Break 3600 MPa
522000 psi
ASTM D3379-100
Elongation at Break 1.4 - 1.8 %
1.4 - 1.8 %
ASTM D3379-75
Modulus of Elasticity 225 GPa
32600 ksi
ASTM D3379-100
Electrical Properties Metric English Comments
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
Descriptive Properties Value Comments
Carbon Content, wt % >95
Mean Fiber Length, mm 0.135
Milled