Material Notes:
This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D 792
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Thickness 3.20 mm
0.011 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm

@Thickness 3.20 mm
0.010 - 0.012 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.0 MPa
9860 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 40 %
40 %
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 103 MPa
14900 psi
2.6 mm/min, 100 mm span; ASTM D 790
Flexural Modulus 2.48 GPa
360 ksi
2.6 mm/min, 100 mm span; ASTM D 790
Izod Impact, Notched 1.86 J/cm

@Temperature 23.0 °C
3.48 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Impact Test 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
53.0 J

@Temperature 23.0 °C
39.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 204 °C

@Thickness 6.40 mm
399 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C

@Thickness 6.40 mm
295 °F

@Thickness 0.252 in
unannealed; ASTM D 648