SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use temperature requirements as defined by UL 1581. 89 Shore A hardness. Good processing by using standard extrusion equipment. UL1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 250 °C
20 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
30S reading; ASTM D2240
Tensile Strength at Break 15.0 MPa
2180 psi
50 mm/min; ISO 527
16.0 MPa
2320 psi
Type I, 50 mm/min; ASTM D638
18.0 MPa
2610 psi
UL 1581
21.0 MPa
3050 psi
after 7days @113°C; UL 1581
Elongation at Break 160 %
160 %
after 7days @113°C; UL 1581
170 %
170 %
Type I, 50 mm/min; ASTM D638
215 %
215 %
UL 1581
Elongation at Yield 140 %
140 %
50 mm/min; ISO 527
Flexural Modulus 0.140 GPa
20.3 ksi
12.5 mm/min; ISO 178
0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
Tear Strength 7.00 kN/m
39.9 pli
ISO 6383
Heat Distortion 9.0 %

@Load 0.250 kg,
Temperature 100 °C
9.0 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
UL 94 by SABIC-IP
Oxygen Index 27 %
27 %
ISO 4589
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
ASTM D257
Surface Resistance 5.10e+15 ohm
5.10e+15 ohm
ASTM D257
Dielectric Constant 2.9

@Frequency 1.00e+6 Hz
2.9

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm

@Thickness 2.00 mm
610 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
VW-1 Pass