Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 250 °C
15 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
30S reading; ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
Type I, 50 mm/min; ASTM D638
18.0 MPa
2610 psi
50 mm/min; ISO 527
27.0 MPa
3920 psi
after 7days @136°C; UL 1581
30.0 MPa
4350 psi
UL 1581
Elongation at Break 130 %
130 %
50 mm/min; ISO 527
140 %
140 %
Type I, 50 mm/min; ASTM D638
200 %
200 %
after 7days @136°C; UL 1581
280 %
280 %
UL 1581
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.100 GPa
14.5 ksi
12.5 mm/min; ISO 178
Heat Distortion 20 %

@Load 0.250 kg,
Temperature 121 °C
20 %

@Load 0.551 lb,
Temperature 250 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL temperature rating; UL 1581
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D746
Oxygen Index 28 %
28 %
ISO 4589
Glow Wire Test 825 °C
1520 °F
IEC 60695-2-13
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 2.40e+16 ohm-cm
2.40e+16 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm

@Thickness 1.50 mm
711 kV/in

@Thickness 0.0591 in
in oil; IEC 60243-1
Dissipation Factor 0.0028

@Frequency 1.00e+6 Hz
0.0028

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 143
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 67
ASTM E 662
Users viewing this material also viewed the following: