| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Water Absorption | 0.070 % @Time 86400 sec |
0.070 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.20 mm |
0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 250 °C |
33 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 115 | 115 | ASTM D785 |
| Tensile Strength, Yield | 38.0 MPa | 5510 psi | SABIC - Japan Method |
| Elongation at Break | 80 % | 80 % | SABIC - Japan Method |
| Flexural Strength | 63.0 MPa | 9140 psi | ASTM D790 |
| Flexural Modulus | 2.33 GPa | 338 ksi | ASTM D790 |
| Izod Impact, Notched | 2.61 J/cm | 4.89 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-1 @Thickness 1.47 mm |
V-1 @Thickness 0.0579 in |
UL 94 |
| V-0 @Thickness 6.10 mm |
V-0 @Thickness 0.240 in |
UL 94 | |
| 5VA @Thickness 6.10 mm |
5VA @Thickness 0.240 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |