Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
7 MFR LEXAN HFD Copolymer
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 7.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
7.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
Melt Index of Compound 6.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
6.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 67.0 MPa
9720 psi
Type I, 50 mm/min; ASTM D638
73.0 MPa
10600 psi
50 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa
8410 psi
Type I, 50 mm/min; ASTM D638
60.0 MPa
8700 psi
50 mm/min; ISO 527
Elongation at Break 141 %
141 %
50 mm/min; ISO 527
142 %
142 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.08 GPa
302 ksi
1 mm/min; ISO 527
2.26 GPa
328 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 89.0 MPa
12900 psi
2 mm/min; ISO 178
98.0 MPa
14200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
2 mm/min; ISO 178
2.24 GPa
325 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 9.66 J/cm
18.1 ft-lb/in
ASTM D256
8.99 J/cm
<br>@Temperature -30.0 °C
16.8 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 72.0 kJ/m²
34.3 ft-lb/in²
80*10*3; ISO 180/1A
63.0 kJ/m²
<br>@Temperature -30.0 °C
30.0 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
6.90 J/cm²
<br>@Temperature -30.0 °C
32.8 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 78.0 J
<br>@Temperature 23.0 °C
57.5 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
<br>@Thickness 3.20 mm
257 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
115 °C
<br>@Thickness 3.20 mm
239 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 130 °C
266 °F
Rate B/50; ISO 306
131 °C
268 °F
Rate B/120; ISO 306
136 °C
277 °F
Rate B/50; ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.582
1.582
ASTM D542
Haze <= 1.0 %
<br>@Thickness 2.54 mm
<= 1.0 %
<br>@Thickness 0.100 in
ASTM D1003
Transmission, Visible 88 %
88 %
2.54 mm; ASTM D1003
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASS
IEC 60695-10-2
Copyright © lookpolymers.com All Rights Reserved