Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0070 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS
LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific)
LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific)
LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS
LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS
LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp CI001 PS
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm

@Time 86400 sec
0.0030 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK
LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK
LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm

@Time 86400 sec
0.0030 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK
LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK
LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific)
LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm

@Thickness 0.750 - 2.30 mm
0.0040 - 0.0070 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS
LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS
LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific)
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0070 cm/cm

@Time 86400 sec
0.0060 - 0.0070 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11
LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0070 cm/cm

@Time 86400 sec
0.0060 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6
LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific)
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.
Copyright © lookpolymers.com All Rights Reserved