Material Notes:
LNP* VERTON* MV007U is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilized.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm

@Time 86400 sec
0.0020 - 0.0050 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
5 mm/min; ISO 527
Elongation at Break 1.7 %
1.7 %
5 mm/min; ISO 527
Tensile Modulus 9.80 GPa
1420 ksi
1 mm/min; ISO 527
Flexural Strength 162 MPa
23500 psi
2 mm/min; ISO 178
Flexural Modulus 7.70 GPa
1120 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
324 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Users viewing this material also viewed the following: