Category | Polymer , Thermoplastic , Polycarbonate (PC) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | LNP STAT-KON |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics LNP STAT-KON DE003M PC.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Moisture Absorption | 0.130 % | 0.130 % | 50% RH, 24 hrs; ASTM D570 |
0.210 % | 0.210 % | 23°C / 50% RH; ISO 62 | |
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 100 MPa | 14500 psi | 5 mm/min; ISO 527 |
101 MPa | 14600 psi | Type I, 5 mm/min; ASTM D638 | |
Tensile Strength, Yield | 100 MPa | 14500 psi | 5 mm/min; ISO 527 |
101 MPa | 14600 psi | Type I, 5 mm/min; ASTM D638 | |
Elongation at Break | 2.8 % | 2.8 % | 5 mm/min; ISO 527 |
2.9 % | 2.9 % | Type I, 5 mm/min; ASTM D638 | |
Elongation at Yield | 2.7 % | 2.7 % | 5 mm/min; ISO 527 |
2.8 % | 2.8 % | Type I, 5 mm/min; ASTM D638 | |
Tensile Modulus | 8.04 GPa | 1170 ksi | 1 mm/min; ISO 527 |
8.47 GPa | 1230 ksi | 50 mm/min; ASTM D638 | |
Flexural Strength | 162 MPa | 23500 psi | ISO 178 |
175 MPa | 25400 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Yield Strength | 175 MPa | 25400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Flexural Modulus | 6.84 GPa | 992 ksi | 2 mm/min; ISO 178 |
9.79 GPa | 1420 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 0.730 J/cm | 1.37 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 6.19 J/cm | 11.6 ft-lb/in | ASTM D4812 |
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
Dart Drop, Total Energy | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
1.11 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
CTE, linear, Transverse to Flow | 0.700 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.389 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Deflection Temperature at 0.46 MPa (66 psi) | 148 °C | 298 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
148 °C @Thickness 3.20 mm |
298 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.0 - 5.0 ohm | 3.0 - 5.0 ohm | ASTM D257 |