| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) |
| Manufacturer | Quantum Advanced Engineering Plastics |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quantum PPS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
| Water Absorption | 0.020 % | 0.020 % | ASTM D570 |
| Water Absorption at Saturation | 0.030 % | 0.030 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 95 | 95 | ASTM D785 |
| Hardness, Rockwell R | 125 | 125 | ASTM D785 |
| Hardness, Shore D | 86 | 86 | ASTM 2240 |
| Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
| Elongation at Break | 4.0 - 5.0 % | 4.0 - 5.0 % | ASTM D638 |
| Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
| Flexural Strength | 145 MPa | 21000 psi | ASTM D790 |
| Flexural Modulus | 4.00 GPa | 580 ksi | ASTM D790 |
| Compressive Strength | 145 MPa | 21000 psi | ASTM D695 |
| Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
| Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 52.2 µm/m-°C | 29.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 282 °C | 540 °F | ASTM D3417 |
| Maximum Service Temperature, Air | 218 °C | 425 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 4.50e+16 ohm-cm | 4.50e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.0 @Frequency 1.00e+6 Hz |
3.0 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
| Dissipation Factor | 0.0010 @Frequency 1.00e+6 Hz |
0.0010 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | no |