| Category | Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled |
| Manufacturer | Quantum Advanced Engineering Plastics |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quantum PEEK 30% Glass Fiber Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
| Water Absorption | 0.10 % | 0.10 % | ASTM D570 |
| Water Absorption at Saturation | 0.30 % | 0.30 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 105 | 105 | ASTM D785 |
| Hardness, Rockwell R | 126 | 126 | ASTM D785 |
| Hardness, Shore D | 85 | 85 | ASTM 2240 |
| Tensile Strength | 165 MPa | 24000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 8.96 GPa | 1300 ksi | ASTM D638 |
| Flexural Strength | 193 MPa | 28000 psi | ASTM D790 |
| Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
| Compressive Strength | 179 MPa | 26000 psi | ASTM D695 |
| Shear Strength | 96.5 MPa | 14000 psi | ASTM D732 |
| Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 21.6 µm/m-°C | 12.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.429 W/m-K | 2.98 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 341 °C | 645 °F | ASTM D3417 |
| Maximum Service Temperature, Air | 266 °C | 510 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | no |