| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO |
| Manufacturer | Quantum Advanced Engineering Plastics |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quantum Modified PPO - Noryl®.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Water Absorption | 0.070 % | 0.070 % | ASTM D570 |
| Water Absorption at Saturation | 0.20 % | 0.20 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength | 64.8 MPa | 9400 psi | ASTM D638 |
| Elongation at Break | 30 % | 30 % | ASTM D638 |
| Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
| Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
| Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
| Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
| Coefficient of Friction | 0.35 | 0.35 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
| Maximum Service Temperature, Air | 104 °C | 220 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | ASTM D648 |
| Flammability, UL94 | V-1 | V-1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 |
| Dissipation Factor | 0.0010 @Frequency 1.00e+6 Hz |
0.0010 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | no |