Material Notes:
Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1000°C. The thermal shock resistance is excellent.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.60 - 2.70 g/cc
0.0939 - 0.0975 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 2.20 - 4.20 W/m-K

@Temperature 1400 °C
15.3 - 29.1 BTU-in/hr-ft²-°F

@Temperature 2550 °F
4.50 - 6.50 W/m-K

@Temperature 600 °C
31.2 - 45.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
5.00 - 7.00 W/m-K

@Temperature 100 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.100 - 0.100 %

@Temperature 1400 °C
-0.100 - 0.100 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 45 %
45 %
Fe2O3 0.20 %
0.20 %
SiC 50 %
50 %
SiO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2600 kg
Mixing Water 4-4.5 liters
per 100 kgs dry material
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved