| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | Qualchem Zrt. |
| Trade Name | Danamid |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Qualchem Danamid AFES-23 Polyamide 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527-1,2 |
| Charpy Impact Unnotched | NB @Temperature -20.0 °C |
NB @Temperature -4.00 °F |
DIN 53453 |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DIN 53453 | |
| Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | HB @Thickness 4.00 mm |
HB @Thickness 0.157 in |
MSZ 10383 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | DIN 53482 |
| Comparative Tracking Index | 400 V | 400 V | IEC 112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 2.0 - 2.2 % | 2.0 - 2.2 % | DIN 53714 |