Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | TIVAR® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.45 g/cc | 1.45 g/cc | ASTM D792 |
Water Absorption | <= 0.010 % | <= 0.010 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | <= 0.010 % | <= 0.010 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 64 | 64 | ASTM D2240 |
Tensile Strength | 19.3 MPa | 2800 psi | ASTM D638 |
Elongation at Break | 125 % | 125 % | ASTM D638 |
Tensile Modulus | 0.421 GPa | 61.0 ksi | ASTM D638 |
Flexural Modulus | 0.752 GPa | 109 ksi | ASTM D790 |
Compressive Strength | 24.8 MPa | 3600 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 0.579 GPa | 84.0 ksi | ASTM D695 |
Coefficient of Friction, Dynamic | 0.14 | 0.14 | Dry vs. Steel; QTM55007 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 127 °C | 260 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+10 ohm | >= 1.00e+10 ohm | ASTM D257 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Limited | Limited | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
Alkalies, Weak | Acceptable | Acceptable | |
Chlorinated Solvents | Acceptable | Acceptable | |
Conductive / Static Dissipative | Yes | Yes | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Limited | Limited |
Descriptive Properties | Value | Comments |
---|---|---|
Machinability | 3 | 1-10, 1=Easier to Machine |