| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Borotron® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quadrant EPP Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.01 g/cc | 1.01 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 71 | 71 | ASTM D2240 |
| Tensile Strength | 16.60 MPa | 2407 psi | ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 0.7667 GPa | 111.2 ksi | ASTM D638 |
| Flexural Strength | 29.1 MPa | 4220 psi | ASTM D790 |
| Flexural Modulus | 0.8729 GPa | 126.6 ksi | ASTM D790 |
| Compressive Strength | 6.60 MPa | 957 psi | 10% Def.; ASTM D695 |
| 11.70 MPa | 1697 psi | 2% Def.; ASTM D695 | |
| 19.1 MPa | 2770 psi | 5% Def.; ASTM D695 | |
| 24.50 MPa | 3553 psi | 10% Def.; ASTM D695 | |
| Compressive Modulus | 0.6718 GPa | 97.44 ksi | ASTM D695 |
| Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 198 µm/m-°C @Temperature -40.0 - 150 °C |
110 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
| Melting Point | 128 °C | 262 °F | ASTM D3418 |
| Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Acceptable | Acceptable | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Unacceptable | Unacceptable | |
| Conductive / Static Dissipative | Yes | Yes | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Unacceptable | Unacceptable | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Unacceptable | Unacceptable |