Epoxy Technology EPO-TEK® OM125 Optical Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Epoxy Technology
Trade Name EPO-TEK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxy Technology EPO-TEK® OM125 Optical Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: EPO-TEK® OM125 is two component, high Tg, optical epoxy designed for bonding multi-mode fiber optic connectors. Advantages & Application Notes: Color coded blue for easy operator ID on the manufacturing floor.A reliability test report is available when using MM fibers and MT ferrule connectors.It is compatible with Telcordia GR1221 and GR326.Versatility in curing from 23°C to 80°C. When used in optical beam pathway, a non-blue version is available. A low viscosity allows for wicking and capillary process methods. Can also be used for potting and encapsulation.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
Part B
1.16 g/cc
1.16 g/cc
Part A
Viscosity 2400 - 5400 cP

@Temperature 23.0 °C
2400 - 5400 cP

@Temperature 73.4 °F
50 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Tensile Modulus 2.67 GPa
388 ksi
Storage
Shear Strength 5.57 MPa
808 psi
Lap
>= 46.9 MPa
>= 6800 psi
Die
Thermal Properties Metric English Comments
CTE, linear 28.0 µm/m-°C
15.6 µin/in-°F
Below Tg
114 µm/m-°C
63.3 µin/in-°F
Above Tg
Maximum Service Temperature, Air 175 °C
347 °F
Continuous
275 °C
527 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 80.0 °C
>= 176 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 367 °C
693 °F
Degradation Temperature
Optical Properties Metric English Comments
Transmission, Visible >= 96 %

@Wavelength 1500 nm
>= 96 %

@Wavelength 1500 nm
Spectral
>= 97 %

@Wavelength 800 nm
>= 97 %

@Wavelength 800 nm
Spectral
>= 98 %

@Wavelength 1000 nm
>= 98 %

@Wavelength 1000 nm
Spectral
Electrical Properties Metric English Comments
Volume Resistivity <= 2.00e+13 ohm-cm
<= 2.00e+13 ohm-cm
Dielectric Constant 3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
Dissipation Factor 0.0188

@Frequency 1000 Hz
0.0188

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 80.0 °C
1.00 hour

@Temperature 176 °F
Minimum Bond Line
120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
Minimum Bond Line
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Minimum Bond Line
Pot Life <= 60 min
<= 60 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Blue
Part B
Clear/Colorless
Part A
Consistency Pourable liquid
Mix Ratio By Weight 10:3
Number of Components Two
Weight Loss 0.25%
200°C
0.56%
250°C
1.43%
300°C