Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.10 - 1.70 GPa | 160 - 247 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Modulus of Elasticity | 1.10 - 1.70 GPa | 160 - 247 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8530_Gray60 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |