Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Protective Coating PC-11® White Epoxy Paste

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Protective Coating Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Protective Coating PC-11® White Epoxy Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC-11® formulation provides working time of over 1/2 hour, giving user ample time to complete larger jobs, reposition work or make changes. PC-11® demonstrates excellent chemical resistance to mild acids, caustics, detergents, gasoline, fuel oil, salt and fresh water. PC-11® will not bond to TEFLON®, polyethylene, and some soft flexible plastics.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Water Absorption 0.44 %
0.44 %
ASTM C413
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
1 Week Cure; ASTM D2240
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 17.69 MPa
2565 psi
ASTM D580
Compressive Strength 32.30 MPa
4685 psi
ASTM D695
Adhesive Bond Strength 11.8 MPa
1710 psi
Tensile Shear Strength; ASTM D1002
Gardner Impact 16.0 J
11.8 ft-lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Users viewing this material also viewed the following: