Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PREWHITE PE 18-50

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Premix Thermoplastics Inc.
Trade Name PREWHITE
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Premix Thermoplastics PREWHITE PE 18-50.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PREWHITE PE 18-50 is a polyethylene based white masterbatch, developed for demanding extrusion coating applications. High processing temperatures and dosing levels are possible without a risk for lacing, die-lip oxidation. Line speeds exceeding 400m/min can be used.According to FDA and BgVV regulations PREWHITE PE 18-50 is approved for use in contact with foodstuffs without limitations.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Additive Loading 50 %
50 %
TiO2 (rutile)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 320 °C
608 °F
30% Masterbatch
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Carrier PE-LD
Dosing, % 30 max
Predrying at 3 hours at 90°C is recommended
Light Fastness 8-Very Good