Polyram RamOfin PL108 LUBRICATED COMPUND FOR PIPES DUCTING, Lubricated

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PL108 LUBRICATED COMPUND FOR PIPES DUCTING, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lubricated polyethylene specially developed for optical fiber communication pipesInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
DIN 53479
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM-D638
Elongation at Break >= 300 %
>= 300 %
ASTM-D638
Tensile Modulus 0.390 GPa
56.6 ksi
ASTM-D790
Izod Impact, Notched 5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Coefficient of Friction 0.050
0.050
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in