Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Filler Content 15 %
15 %
±2%; Polykemi
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
With Flow; ISO 2577
0.0090 cm/cm
0.0090 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 79

@Time 15.0 sec
79

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break <= 130 MPa
<= 18900 psi
ISO/R527
Elongation at Break 3.5 %
3.5 %
ISO/R527
Flexural Strength <= 190 MPa
<= 27600 psi
ISO 178
Flexural Modulus 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179
0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
120°C/h; ISO 75/1
Vicat Softening Point >= 200 °C

@Load 5.001 kg
>= 392 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
IEC 695-2-1