PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.546 g/cc
1.546 g/cc
ASTM D792
Linear Mold Shrinkage 0.0041 cm/cm
0.0041 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.17 MPa
5391 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 0.7152 %
0.7152 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 10.31 GPa
1495 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 70.292 MPa
10195 psi
ASTM D790
Flexural Modulus 7.888 GPa
1144 ksi
ASTM D790
Izod Impact, Notched 0.246 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.461 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity >= 36.99 W/m-K
>= 256.7 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Surface Resistivity per Square 110000 ohm
110000 ohm
ASTM D257
Descriptive Properties Value Comments
Product Form Pellets
Users viewing this material also viewed the following: