PolyOne Syncure™ V0044G-UV RoHS Natural Polyethylene, Crosslinked (XLPE)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer PolyOne Corporation
Trade Name Syncure™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Syncure™ V0044G-UV RoHS Natural Polyethylene, Crosslinked (XLPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System S110FV-UV.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 2.24 g/cc
2.24 g/cc
ASTM D792
Density 1.25 g/cc
0.0452 lb/in³
Geon® 1169; Internal Method
Melt Flow 3.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Descriptive Properties Value Comments
Agency Ratings UL 4703
Features Flame Retardant
Sunlight Resistant (720 hours)
Forms Pellets
Generic Material XLPE
Generic Name Polyethylene, Crosslinked (XLPE)
Regional Availability North America
RoHS Compliance RoHS Compliant
Uses Wire & Cable Applications