Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable WJJC340 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable WJJC340 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
15 sec; ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 270 %
270 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Oxygen Index 31 %

@Thickness 1.91 mm
31 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 171 - 188 °C
340 - 370 °F
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 88%
ASTM D638; 100°C, 762.0 µm; 240 hr, UL Standard
Retention of Tensile Strength 110%
ASTM D638; 100°C, 762.0 µm; 240 hr, UL Standard
RoHS Compliance RoHS Compliant
Uses Cable Jacketing
Wire & Cable Applications