PolyOne Geon™ Vinyl Wire & Cable W3201 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable W3201 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Geon® W3201 is UL recognized for UL 94 V0 per QMFZ2, and is suitable for injection molding. This product meets UL 105°C, AWM, and Mil-W-76 80°C insulation.NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Yield 16.2 MPa
2350 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 290 %
290 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -26.0 °C
-14.8 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 1.90 mm
V-0

@Thickness 0.0748 in
ALL; UL 94
Oxygen Index 25 %

@Thickness 1.91 mm
25 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 182 - 188 °C
360 - 370 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings MIL W-76
UL QMFZ2
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 95%
136°C, 1.91 mm; 168 hr, UL Standard
Uses Flexible Cord Insulation
Insulation
Wire & Cable Applications
Wire Types AWM