| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 5.86 MPa @Strain 100 % |
850 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| PolyOne Geon™ HC 2165 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2165 is a 65 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2165 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
| Tensile Strength | 5.86 MPa @Strain 100 % |
850 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| PolyOne Geon™ HC 2165G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2165G is a 65 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2165G can be used for extrusion and injection molding healthcare applicatio.. |
|||
| Tensile Strength | 5.86 MPa @Strain 100 % |
850 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| PolyOne Geon™ Vinyl Flexible A7501 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
| Tensile Strength | 5.86 MPa @Strain 100 % |
850 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| PolyOne Geon™ Vinyl Flexible A7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
| Tensile Strength | 5.86 MPa @Strain 100 % |
850 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
| Tensile Strength | 5.86 MPa | 850 psi | |
| Teknor Apex Elexar® EL 3954-70 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | |
| Teknor Apex Tekbond® TB 2020A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
| Tensile Strength | >= 5.86 MPa | >= 850 psi | Compound Property |
| Arlon 30540R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier This data represents typical values for the production material. The data should not be used to write, or in plac.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production ma.. |
|||
| Tensile Strength | >= 5.86 MPa | >= 850 psi | Compound Property |
| Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material.. |
|||
| Tensile Strength | >= 5.86 MPa | >= 850 psi | Compound Property, Side 1 |
| Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property |
| Arlon 51191R014 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the .. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic.. |
|||
| Tensile Strength | >= 5.86 MPa | >= 850 psi | Compound Property |
| Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |
|||
| Tensile Strength | 5.86 MPa | 850 psi | Silicone Property; ASTM D412 |
| Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty.. |
|||