Polymer Property : Tensile Strength = 1200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A85UB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B87FB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R8570A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV 3450 Polyvinyl Chloride, Flexible (PVC, Flexible)
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of..
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3881 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B4DC1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.27 MPa
1200 psi
Typical
Garlock 2564 C.I. NBR/CR/SBR Sheet Rubber, Polyester Insert
Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2264 is a smooth fini..
Tensile Strength 8.27 MPa
1200 psi
Typical
Garlock 363 Nitrile Sheet Rubber
Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #363 is a good quality, oil-resistant nitrile sheet.Information provided by Garlock Rub..
Tensile Strength >= 8.27 MPa
>= 1200 psi
Garlock 4160 Natural Sheet Rubber
Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Red, smooth finishInformation provided by Garlock Rubber Technologies
Tensile Strength 8.27 MPa
1200 psi
Typical
Garlock 567 EPDM Sheet Rubber
Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish, commercial qualityInformation provided by Garlock Rubber Technologi..
Tensile Strength 8.27 MPa
1200 psi
ASTM F152
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u..
Tensile Strength 8.27 MPa
1200 psi
ASTM F152
Garlock THERMA-PURâ„¢ 4122-KAMM High Temperature Gasketing Material
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u..
Tensile Strength 8.27 MPa
1200 psi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1117 P (SIS) Linear Triblock Copolymer
Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: ..
Tensile Strength 8.30 MPa
1200 psi
Flatwise
Henkel Hysol EA 9695 Film Adhesive
Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 ps..
Tensile Strength 8.30 MPa
1200 psi
Momentive Performance Materials FSE7540 Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 8.27 MPa
1200 psi
ASTM D638
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE
F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru..
Tensile Strength 8.30 MPa
1200 psi
Shin-Etsu Silicones LIMSâ„¢ KE2095-60AB Elastomer
KE-2095-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Tensile Strength 8.27 MPa
1200 psi
Teknor Apex Tekbond® TB 1416A Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Tensile Strength 8.27 - 10.3 MPa
1200 - 1500 psi
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy
Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre..
Tensile Strength 8.30 MPa
1200 psi
ASTM D412
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer
Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for ..
Tensile Strength 8.30 MPa
1200 psi
ASTM D412
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer
Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer..
Tensile Strength 8.27 MPa
1200 psi
Silicone Property; ASTM D412
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate..
Tensile Strength 8.27 MPa
1200 psi
Silicone Property; ASTM D412
Arlon LW401A##-P3 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Blue, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length ..
Tensile Strength 8.27 MPa
1200 psi
Silicone Property; ASTM D412
Arlon R34581R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents ty..
Tensile Strength 8.27 MPa
1200 psi
AlphaGary AlphaSeal™ 04-073 P Modified Thermoplastic Elastomer
AlphaSeal™ 04-073 P Modified is a TPE based material recommended for injection molded corks. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resista..
Tensile Strength >= 8.27 MPa
>= 1200 psi
Compound Property
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
Tensile Strength 8.27 MPa
1200 psi
ASTM D412
Arlon SFT 0.012" (0.305 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: PET Product: Cured Self-Fusing Silicone Rubber Cross-Section: 1” Wide RectangularDescription: 1 inch wide, 12 mil thick x 10 yards long, Gray, Rectangular cross-sec..
Tensile Strength 8.27 MPa
1200 psi
ASTM F152
Garlock THERMA-PUR™ 4122-FC High Temperature Gasketing Material
THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a uniqu..