PolyOne Geon™ Vinyl Flexible 90043 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible 90043 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Volatiles 0.30 %

@Thickness 1.91 mm,
Temperature 105 °C
0.30 %

@Thickness 0.0752 in,
Temperature 221 °F
Loss; Method A; ASTM D1203B
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
15 sec; ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
510 mm/min; ASTM D638
Elongation at Break 320 %
320 %
510 mm/min; ASTM D638
Tear Strength 62.3 kN/m
355 pli
Die C, 2 in/min; ASTM D1004
Descriptive Properties Value Comments
Automotive Specifications CHRYSLER MS-DC211 Type B
CHRYSLER MS-DC211 Type B CPN2713 Color: 100% Color Match
GM GMP.PVC.010
Features High Gloss
Forms Pellets
Fungal Resistance Pass
ASTM G21
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Low Temperature Flexibility Pass
-29°C, 508.0 µm; 4 hr, 12 mm
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Exterior Trim
Outdoor Applications
Xenon Weatherometer Pass
SAE J1960; Exterior, 301 kJ/m², All Colors, dE*<3.0