PolyOne Aquamix™ 568 Latex

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer PolyOne Corporation
Trade Name Aquamix™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne Aquamix™ 568 Latex.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersability, and other physical properties. Any soft settling may be removed by stirring. Copies of PolyOne test methods are available upon customer request.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid
Solids Content 51 - 53 %

@Temperature 105 °C
51 - 53 %

@Temperature 221 °F
Particle Size <= 5.0 µm
<= 5.0 µm
pH 8.0 - 10
8.0 - 10
Brookfield Viscosity 400 - 1000 cP
400 - 1000 cP
RVF #3, 10 rpm, 424
Descriptive Properties Value Comments
Active Ingredient Polypale Ester 10 BHT with ~softening point 109°C
Binder/Vehicle Water
Forms Pellets
Generic Material Latex
Generic Name Latex
Regional Availability North America