| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Brookfield Viscosity | 400 cP | 400 cP | 20 rpm; ASTM D1417 |
| Polimeri Europa Europrene Latice® 5584 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 5584 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Eu.. |
|||
| Brookfield Viscosity | 400 cP | 400 cP | 20 rpm; ASTM D1417 |
| Polimeri Europa Europrene Latice® 5595 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 5595 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers.Key Features: Europrene Latice® 5595 is specifically des.. |
|||
| Brookfield Viscosity | 400 cP @Temperature 25.0 °C |
400 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
| Omya HYDROCARB® 95 HS Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
| Brookfield Viscosity | 400 - 1000 cP | 400 - 1000 cP | RVF #3, 10 rpm, 424 |
| PolyOne Aquamix™ 568 Latex Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit.. |
|||
| Brookfield Viscosity | 400 cP | 400 cP | One Day Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method |
| PolyOne Geon™ 170 Series 178 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 178 is a high molecular weight, fine particle size homopolymer dispersion resin. It provides the ability to produce thin gauge coatings. It is recommended for applications such as food and be.. |
|||
| Brookfield Viscosity | 400 - 800 cP @Temperature 20.0 °C |
400 - 800 cP @Temperature 68.0 °F |
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A |
| Lubrizol Advanced Materials Pearlstick® 45-50/05 Linear Thermoplastic Polyurethane Elastomer
(discontinued ** Pearlstick 45-50/05 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-.. |
|||
| Brookfield Viscosity | 400 - 1200 cP | 400 - 1200 cP | #2/20 rpm |
| Mallard Creek Polymers BarrierPro® 4545 SBR Emulsion BARRIER PRO® 4545 is an anionic carboxylated styrene-butadiene copolymer latex. Features: highly stable, good compatibility with fillers and pigments, etc., cured films are tough and pliable, cur.. |
|||
| Brookfield Viscosity | <= 400 cP | <= 400 cP | #2/20 rpm |
| Mallard Creek Polymers ROVENE® 18106 Styrene-Acrylic Emulsion ROVENE® 18106 is a styrene-acrylic copolymer emulsion. This latex provides good water resistance together with good grease resistance. ROVENE® 18106 exhibits excellent mechanical stability and.. |
|||
| Brookfield Viscosity | <= 400 cP | <= 400 cP | #20/200 rpm |
| Mallard Creek Polymers ROVENE® 6023 Carboxylated Acrylic Copolymer Latex Applications: Rovene® 6023 in portland cement mixtures results in increased adhesion to most substrates, improved water resistance, increased flexural strength and good resistance to UV light. Ro.. |
|||
| Brookfield Viscosity | 400 cP | 400 cP | #2/20 rpm |
| Mallard Creek Polymers ROVENE® 6066 Styrene-Acrylic Latex Applications: Rovene® 6066 is specifically designed for formulation of binder systems for moldable and self supporting composites. Its molecular weight allows formulation latitude for many ‘.. |
|||
| Brookfield Viscosity | 400 - 1000 cP | 400 - 1000 cP | #2/20 rpm |
| Mallard Creek Polymers ROVENE® 6087 Styrene-Acrylic Emulsion ROVENE® 6087 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.APPLICATIONS: ROVENE® 6087 typical applications.. |
|||
| Brookfield Viscosity | 400 - 1000 cP | 400 - 1000 cP | #20/200 |
| Mallard Creek Polymers Rovene® 6102 Resin Supported Emulsion Rovene® 6102 is a hard, film forming vehicle with a moderately low glass transition temperature (Tg) for flexographic and gravure inks and overprint varnishes, that exhibits good water resistance.. |
|||
| Brookfield Viscosity | 400 - 1000 cP | 400 - 1000 cP | #2/20 rpm |
| Mallard Creek Polymers ROVENE® 6487 Styrene-Acrylic Emulsion ROVENE® 6487 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.APPLICATIONS: ROVENE® 6487 typical applications.. |
|||
| Brookfield Viscosity | <= 400 cP | <= 400 cP | #2/20 rpm |
| Mallard Creek Polymers ROVENE® 9423 SBR Latex ROVENE® 9423 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight and styren.. |
|||
| Brookfield Viscosity | 400 - 1000 cP | 400 - 1000 cP | #20/200 |
| Mallard Creek Polymers Tykote® 6152 Styrene-Acrylic Emulsion Tykote® 6152 is a hard film forming styrene-acrylic emulsion designed for oil and grease resistant barrier coatings. This product also provides excellent water and blocking resistance in barrier .. |
|||
| Brookfield Viscosity | 400 - 800 cP | 400 - 800 cP | Spindle # 3, rpm 60 |
| Michelman® HydroGrease White™ 22 White coating Description: High performance water and grease resistant white coatingUsage: HydroGrease White™ 22 is a white coating which imparts water and grease resistance to the substrate. This coating is.. |
|||
| Brookfield Viscosity | 400 - 700 cP | 400 - 700 cP | Spindle # 3, rpm 60 |
| Michelman® Michem® Coat 82 Water resistance coating Description: Water resistance coating with intermediate moisture barrier and higher COF.Usage: Michem® Coat 82 is a repulpable, printable, and cold set gluable coating optimized for water resista.. |
|||
| Brookfield Viscosity | 400 - 1800 cP | 400 - 1800 cP | Spindle # 3, rpm 60 |
| Michelman® Michem® Emulsion 34935 Anionic paraffin/ethylene acrylic acid wax emulsion Description: Anionic paraffin/ethylene acrylic acid wax emulsionUsage: Michem® Emulsion 34935 is best used as an additive where excellent water beading properties are required It is primarily use.. |
|||
| Brookfield Viscosity | 400 cP | 400 cP | ASTM D2196-66; LVT, Spindle #2 @ 30rpm |
| Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |
|||
| Brookfield Viscosity | 400 cP | 400 cP | ASTM D2196, LVT, Spindle #2 @ 30rpm |
| Lord Adhesives Chemglaze® V175 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
| Brookfield Viscosity | 400 - 3200 cP | 400 - 3200 cP | Spindle # 4, rpm 60 |
| Michelman® Michem® Lube 124 Anionic microcrystalline wax emulsion Description: Anionic microcrystalline wax emulsionUsage: Michem® Lube 124 as an additive provides release and acts as a detackifier for synthetic and natural rubber. Michem® Lube 124 is used s.. |
|||
| Brookfield Viscosity | 400 - 600 cP | 400 - 600 cP | Spindle # 3, rpm 60 |
| Michelman® VaporCoat® 330C Topical MVTR Description: Topical MVTR and water resistance coatingUsage: VaporCoat® 330C is a repulpable, printable and cold set gluable moisture vapor coating. Common uses for VaporCoat® 330C include rol.. |
|||
| Brookfield Viscosity | 400 - 530 cP @Temperature 25.0 °C |
400 - 530 cP @Temperature 77.0 °F |
25% Toluene solution |
| Kraton® G1652 E (SEBS) Linear Block Copolymer Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
| Brookfield Viscosity | 400 - 6000 cP @Temperature 25.0 °C |
400 - 6000 cP @Temperature 77.0 °F |
25% solution in Toluene |
| Sibur DST-30R-01 2nd Group Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE) Kraton D 1184, 1186. As modifiers for bitumen for production of roofing materials, footwear compositions, adhesives, and coverings, as well as for modification of plastics. Addition of thermal ela.. |
|||
| Brookfield Viscosity | 400 cP @Temperature 25.0 °C |
400 cP @Temperature 77.0 °F |
0.2; MA 04-3-064 |
| Dynasol Calprene® H6140 Hydrogenated Rubber SEBS Calprene H 6140 is a 69/31 Ethylene-Butylene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure with excellent ozone resistance.This product is available in:CH 61.. |
|||
| Brookfield Viscosity | 400 - 1100 cP | 400 - 1100 cP | RVF 3# sp @ 30 rpm, RT |
| 3M 1000NF Fast Tack Water Based Adhesive 3M™ Fast Tack Water Based Adhesive 1000NF is a high performance water-based, one part adhesive formulated for fast bonding and long term heat resistant bonds.Information provided by 3M |
|||
| Brookfield Viscosity | 400 - 800 cP | 400 - 800 cP | RVT #2 spindle @ 20 rpm |
| 3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
| Brookfield Viscosity | 400 - 600 cP | 400 - 600 cP | LVF #2 spindle @2.5 rpm |
| 3M Scotch-Weld™ RT41 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
| Brookfield Viscosity | 400 - 600 cP | 400 - 600 cP | RVT #2 sp @ 20 rpm |
| 3M Scotch-Weld™ TL71 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
| Brookfield Viscosity | 400 cP | 400 cP | 0.1; MA 04-3-064 |
| Dynasol Calprene® H6144 Hydrogenated Rubber (SEBS) Calprene H6144 is a 69/31 ethylene-butylene/styrene thermoplastic copolymer, polymerized in solution and having a linear structure with excellent ozone resistance. Applications: Technical Compoundin.. |
|||