Polimeri Europa Riblene® MM 20 Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MM 20 Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Riblene MM 20 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 are characterized by a high flexibility.Main Applications: Riblene MM 20 is suitable for injection molding, compound and masterbatch applications. Riblene MM 20 is recommended for caps, closures, houseware and high thickness articles.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ISO 868/A
Tensile Strength, Yield 11.0 MPa
1600 psi
ISO 527
Flexural Modulus 0.130 GPa
18.9 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
Internal method
Vicat Softening Point 90.0 °C

@Load 1.00 kg
194 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746