Oceanchem Group Brominated Epoxy Oligomers-2 (BEP-2)

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Epoxy
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Brominated Epoxy Oligomers-2 (BEP-2).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Molecular Formula: (C36H32Br8O6)nCas No.: 68928-70-1Application: BEP-2 is a high molecular weight brominated epoxy polymeric flame retardant designed for a broad range of thermoplastic applications. BEP-2 is recommended for thermoplastic polyesters (PBT, PET), thermoplastic polyurethanes (TPU), alloys (PC/ABS), styrenics (ABS, HIPS) and others. The specially selected molecular weight and the chemical structure of BEP-2 offers high thermal stability and thermal ageing, excellent processability, non-blooming, and good UV stability. BEP-2 offers a similar combination of properties to that of BEP-2 for those applications where higher melt flow (MFI) values are required.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Thermal Properties Metric English Comments
Softening Point 135 - 145 °C
275 - 293 °F
Descriptive Properties Value Comments
Appearance Light Yellow Powder
Bromine, Br (%) >52
CAS Number 68928-70-1
Molecular Formula (C36H32Br8O6)n
Weight Loss (%) 1
332°C
10
353°C
5
339°C