Material Notes:
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their performance under specific conditions. The manufacturing process for each grade is tightly controlled to produce materials that have a uniform microstructure and the right balance of strength, grain size and hardness to offer optimum performance for their intended applications.
Physical Properties Metric English Comments
Apparent Bulk Density 3.12 g/cc
0.113 lb/in³
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Yield 65.0 MPa
9430 psi
Estimated at 70% of flexural strength
Flexural Strength 117 MPa
17000 psi
Compressive Strength 210 MPa
30500 psi
Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C
4.72 µin/in-°F
Thermal Conductivity 175 W/m-K
1210 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000270 ohm-cm
0.000270 ohm-cm
Descriptive Properties Value Comments
Oxidation Threshold 500°C
Temperature that results in 1% weight loss in 24 hours. Oxidation threshold increases by approximately 100°C if graphite is purified.