Material Notes:
PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not recommended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.267 %
0.267 %
ASTM D570
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 82
82
ASTM D785
Tensile Strength, Ultimate 61.0 MPa
8850 psi
ASTM D638
Elongation at Break 0.91 %
0.91 %
ASTM D638
Tensile Modulus 8.50 GPa
1230 ksi
ASTM D638
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Compressive Strength 189 MPa
27400 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 3.15 GPa
457 ksi
Calculated
Izod Impact, Notched 0.166 J/cm
0.311 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.178 J/cm²
0.847 ft-lb/in²
ASTM D256
Impact 100
100
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.510 W/m-K

@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 201 °C
394 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 27.5 %
27.5 %
ASTM D2863
Shrinkage 0.269 %
0.269 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+10 ohm-cm
8.00e+10 ohm-cm
ASTM D247
Dielectric Constant 10.2
10.2
ASTM D150
Dissipation Factor 0.061
0.061
ASTM D150
Arc Resistance 137 sec
137 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638