Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LCF30-PES Polyethersulfone, 30% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone, Carbon Fiber Reinforced
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF30-PES Polyethersulfone, 30% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyethersulfone with 30% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D-792
Filler Content 30 %
30 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 325 MPa
47100 psi
ASTM D-638
Elongation at Break 1.0 %
1.0 %
ASTM D-638
Tensile Modulus 36.552 GPa
5301.4 ksi
ASTM D-638
Flexural Strength 300 MPa
43500 psi
ASTM D-790
Flexural Modulus 22.069 GPa
3200.8 ksi
ASTM D-790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 5.07 J/cm
9.50 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 410 °C
770 °F
ASTM D-648
Users viewing this material also viewed the following: