Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom PLASTALEN® T 20 Regranulate Polypropylene reinforced with mineral filler

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTALEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTALEN® T 20 Regranulate Polypropylene reinforced with mineral filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PP regranulate for injection molding with 20% mineral filler. Application for general purposes in all industrial sectors.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
STN EN ISO 1183-1
Filler Content 20 %
20 %
Linear Mold Shrinkage 0.0102 cm/cm
0.0102 in/in
STN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0103 cm/cm
0.0103 in/in
STN EN ISO 294-4
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 50.0 °C
104 - 122 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content <= 0.20 %
<= 0.20 %
STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi