Permabond 801 Cyanoacrylate, High Temperature

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond 801 Cyanoacrylate, High Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber, metal and plastics. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND® cyanoacrylates the ideal adhesives for high speed production lines. Features & Benefits: High temperature resistance Rapid curing Ease of use – no mixing or heat cure 100% reactive, no solvents Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 10 - 15 cP

@Temperature 25.0 °C
10 - 15 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength 19.0 - 23.0 MPa
2760 - 3340 psi
ISO 4587, Shear
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 132 °C
270 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
0.167 - 0.250 min
0.00278 - 0.00417 hour
Buna N Rubber, handling time
0.167 - 0.250 min
0.00278 - 0.00417 hour
Phenolic, handling time
1440 min
24.0 hour
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.05
Strength Retention 100% at 0°C
Relative to 0°C
60% at 100°C
Relative to 0°C
75% at -50°C
Relative to 0°C
95% at 50°C
Relative to 0°C